- Mixture of cellulose triacetate and diacetate
- Low static charge and high strength
- Enhanced recovery of fastidious gram positive organisms
May be repeatedly sterilized without loss of
integrity or change in bubble point
- Relative to nitrocellulose:
improved solvent resistance to low molecular weight
alcohols
- better heat resistance
- lower protein binding
|
| Cellulose Acetate |
More
properties and specifications
Chemical compatibility |
Available Formats: (click on type for ordering information)
| Types |
Colors |
pore sizes in µm |
diameters in mm |
33cm x 10m |
| 13 |
25 |
37 |
47 |
50 |
82 |
85 |
90 |
142 |
293 |
293/59 |
| Sterile |
White |
0.45 |
- |
- |
- |
l |
- |
l |
l |
- |
- |
- |
- |
- |
| Nonsterile |
White |
0.20 |
l |
l |
l |
l |
- |
l |
- |
l |
l |
l |
l |
l |
| 0.45 |
l |
l |
l |
l |
l |
l |
- |
l |
l |
l |
l |
l |
| 0.80 |
l |
l |
l |
l |
- |
l |
- |
l |
l |
l |
l |
l |
| 3.0 |
l |
l |
- |
l |
l |
- |
- |
l |
l |
l |
l |
- |
Return to Membranes List
| Contact | Catalog | Search
|